Understanding O-Rings: The Key to a Leak-Free Camlock Connection

Share This Post

The gasket is the only part of a camlock that seals, and it is the part most often chosen by habit rather than by specification. Four materials cover almost every duty, and each has a fluid and temperature envelope.

The Four Gasket Materials

Material Good for Avoid Temperature guide
NBR (nitrile) Water, oil, diesel, air Strong solvents, ozone, sunlight −30 to 100°C
EPDM Water, steam, many acids and bases Mineral oils, fuels −40 to 120°C
Viton (FKM) Fuels, aromatics, acids, heat Ketones, some esters −20 to 200°C
PTFE Broad chemical resistance, food contact High-pressure cold flow (use encapsulated) −50 to 230°C

These are working guides, not a chemical compatibility chart. For an aggressive or mixed stream, send the fluid, concentration and temperature and we will confirm the gasket.

Why O-Rings Fail

  • Swelling — the wrong material absorbing the fluid. The gasket grows, will not sit in the recess, and gets pinched on closing.
  • Hardening — heat or chemical attack. The rubber loses elasticity and stops sealing at low pressure.
  • Flattening — compression set after long service. The gasket takes a permanent set and leaks when the joint is remade.
  • Cuts and nibbles — grit in the groove, or an adapter forced past a misaligned gasket.
  • Extrusion — pressure pushing a soft gasket through a gap, usually at high pressure or high temperature.

Replacing a Gasket

  1. Depressurise and drain the line.
  2. Open the cam arms and separate the halves.
  3. Pick the old gasket out with a plastic tool — not a screwdriver, which scores the seat.
  4. Clean the recess; any grit left will cut the new gasket.
  5. Seat the new gasket flat, without twisting.
  6. Close the arms and test at working pressure with soap solution.

Choosing Between NBR and Viton

For water, air and diesel, NBR is the default and the cheapest. Move to Viton when the fuel is aromatic, the temperature is high, or the line sees aggressive chemistry. For food and pharmaceutical duty, use a food-grade EPDM or PTFE gasket and keep the documentation with the line.

Stock Advice

Gaskets are consumables. Keep a set for every size in service, in the material that line actually uses, and replace them at the annual service even if they still look serviceable. A gasket costs a fraction of the downtime from a failed joint.

All four materials are available for every size we supply, from 1/2″ to 6″. See the camlock fitting range or ask us to match a gasket to your fluid.